The least corrosive the soil is, the higher the polarization resistance of the steel pipe.

Source: Funtay / Dreamstime.com

Pipelines are an essential infrastructure component as a conveyance of utilities, commodities and other elements vital for a robust economy. Pipelines are typically constructed from metal, and are prone to corrosion if not well protected and treated. Corrosion is understood as a disintegration of metal through one or more electrochemical processes and/or unintended exposure to chemicals. It usually initiates at the surface where it interfaces with external substrates. (Learn more about these processes in the article Corrosion Electrochemistry: The 6 Electrochemical Reactions Involved in Corrosion.)

Advertisement

Several studies have been conducted to understand pipeline corrosion in various environments. This article describes investigations of pipe specimens in two types of environments: underground/buried in soil and marine/saltwater. In addition, we describe the use of a technique known as electrochemical impedance spectroscopy (EIS) to examine the pipes and their corrosion.

Pipelines in Underground / Buried Environments

The fundamental cause of the deterioration of buried pipelines is soil corrosion. (Learn more about this topic in the article An Introduction to Soil Corrosion.) All metals exhibit a tendency to be oxidized, some more easily than others. Chemically, when metal atoms are exposed to an environment containing water molecules, they release electrons and become positively charged ions. This effect can be concentrated locally to form a pit or a crack, or it can extend across a wide area to produce general deterioration.

Advertisement

The corrosion of buried steel pipes in soil is mainly driven by the soil's properties such as soil resistivity, redox potential, pH, organic content, microbial activity, temperature and chemical composition. Warmer temperatures force anodic and cathodic reactions that aggravate dissolution of the pipeline. In acidic soil, the driving forces for the reaction is fast and results in increased corrosion rates. Corrosion of metals is typically associated with the development of negative voltage caused by the release of electrons.

Comparing electrochemical impedance spectroscopy (EIS) and dynamic electrochemical impedance spectroscopy (DEIS)

Electrochemical impedance spectroscopy (EIS) determines the dielectric properties of materials, as measured by an external field’s interaction with the dipole moment of a particular sample, usually stated by permittivity. A potentiostat is used to conduct EIS measurements. Dynamic electrochemical impedance spectroscopy (DEIS) uses an AC signal while sweeping the potential, and is a powerful method to study the reaction mechanisms of surface electrochemical reactions. Its ability to reliably measure low frequencies while sweeping is key to its successful implementation.

Experimental results

An experiment to investigate underground pipe corrosion was conducted on mild steel pipe specimens. The specimens were cut to a desired dimension and cleaned mechanically and chemically. Three different soils were used as a medium for seven months. The experiment also used three conventional electrode cells as a counter electrode, a saturated calomel electrode (SCE) as a reference electrode, the steel pipe specimens as a working electrode, and an electrolyte as a 3.5% NaCl solution.

Advertisement

EIS measurements and a Tafel polarization test were performed on the steel pipe specimens with a frequency range of 100 KHz to 10 mHz. Results from each soil medium are shown below.

Nyquist curve of steel pipe specimen reaction in soilFigure 1. Nyquist curve of steel pipe specimen reaction in soil #1. The maximum resistance observed is just under 80 ohms.
Source: Electrochemical Corrosion Behavior of Steel Pipe in Alkaline Soil

Advertisement

Nyquist curve of steel pipe specimen reaction in soil Figure 2. Nyquist curve of steel pipe specimen reaction in soil #2. The maximum resistance observed is around 100 ohms.
Source: Electrochemical Corrosion Behavior of Steel Pipe in Alkaline Soil

Nyquist curve of steel pipe specimen reaction in soilFigure 3. Nyquist curve of steel pipe specimen reaction in soil #3. The maximum resistance observed is approximately 150 ohms.
Source: Electrochemical Corrosion Behavior of Steel Pipe in Alkaline Soil

Polarization test results of the 3 soils in 7 monthsFigure 4. Polarization test results of the 3 soils in 7 months.
Source: Electrochemical Corrosion Behavior of Steel Pipe in Alkaline Soil

Discussion analysis

Soil 3 exhibited the highest resistance against corrosion. When tested with Tafel polarization, the result is also consistent with the results shown in Figure 4. This indicates that soil 3 is the least corrosive compared to soil 1 and 2. The polarization test performed on the pipe specimens shows that soil 2 is more corrosive than soil 1, especially in the first 4 months.

The more corrosive the embedded soil is, the higher the degradation rate of metal (steel pipe). The least corrosive the soil is, the higher the polarization resistance of the steel pipe.

Pipelines in the Marine Environment

In seawater, chloride ions usually attack the metal components of the pipeline. This leads to corrosion, which is associated with the localized break down of the pipeline's surface.

Experimental results

A study using dynamic electrochemical impedance spectroscopy (DEIS) was conducted to detect and monitor pitting corrosion of materials. It was carried out under potentiodynamic conditions and had a capability to record the impedance spectra at the point of pitting corrosion.

Typically, stainless steel is used to protect against corrosion in a marine environment. The study used 316L stainless steel and super austenitic stainless steel alloys 33 and 24 as test specimens. (Related reading: 12 Things You Need to Know About Austenitic Stainless Steel.) The specimens were cut to the desired dimension and attached using a brass rod for an electrical connection. Then they were molded with an epoxy-based resin. The specimens were also polished using abrasive paper complete with a diamond paste in order to obtain a scratch-free mirror finish.

Similar to the study described above, a conventional three electrode cell was used for all the electrochemical measurements. A saturated calomel electrode (SCE) was used as a reference electrode, platinum foil as a counter electrode and the test material was a working electrode. Natural sea water was collected to serve as the electrolyte.

Using potentiodynamic studies, there was a capability to record the impedance spectra at the point of pitting corrosion. An analysis was completed using the dynamic electrochemical impedance spectroscopy (DEIS) approach. The DEIS technique was used to evaluate the pitting corrosion resistance of alloys 33 and 24 in natural sea water. The Nyquist plots were used to examine the resistance. The relative corrosion resistance for alloys 33 and 24 in natural seawater showed their higher corrosion pitting resistance (PREN) compared to 316L stainless steel, which may be due to the presence of both nitrogen and molybdenum in the super austenitic alloys.

Share This Article

  • Facebook
  • LinkedIn
  • Twitter
Advertisement

Written by Della Anggabrata

Della Anggabrata

Della is a civil engineer with extensive and progressing experience in a consulting industry with a unique technical skill that combines civil and geotechnical engineering. Her work primarily focuses on underground infrastructure projects in the Lower Mainland of British Columbia, Canada. Some of her projects are large diameter watermains, water and wastewater treatment plants, sanitary forcemains and land development. She is a key contributor to the engineering design and project management, and also provides a solid foundation for every success that the team has achieved.

Della attained a bachelor’s degree of Civil Engineering from the University of British Columbia, Vancouver, where she graduated with a Distinction recognition. In her free time, she is a foodie who cooks, loves travelling and playing tennis. She is always eager to taste and experience new cuisines and recipes.

Related Articles

Go back to top