Abrasion Resistance Testing

Last updated: July 22, 2020

What Does Abrasion Resistance Testing Mean?

Abrasion resistance testing, as its name implies, describes a variety of testing procedures used to measure the abrasion resistance of a solid material. The objective of the test is to produce data that will rank a given material’s resistance to scratching abrasion under a set of specified conditions. Abrasion resistance testing can be performed on a variety of materials, including metals, ceramics, composites and coatings.

In the corrosion industry, abrasion resistance is an essential parameter when selecting protective coatings for metal substrates. Abrasion resistance is also a crucial requirement for warehouse and industrial floors as they are frequently subjected to aggressive actions from trucks and other heavy equipment.

Advertisement

Corrosionpedia Explains Abrasion Resistance Testing

There are several types of abrasion resistance tests, as outlined in various ASTM standards. Some of the most common tests are:

  • Pin abrasion (ASTM G132)
  • Taber abrasion (ASTM D1044, ASTM D4060)
  • Rubber wheel abrasion (ASTM G65)
  • Falling sand abrasion (ASTM D968)
  • RCA abrasion (ASTM F2357)