Luggin Capillary

Last updated: August 15, 2018

What Does Luggin Capillary Mean?

A Luggin capillary is a device used in electrochemistry to transmit a high level of current density on the surface of an electrode in attempts to determine the potential measurement of the electrode.

Advertisement

Corrosionpedia Explains Luggin Capillary

A Luggin capillary is an ideal method used to reduce the distance between the sensor tip of a reference electrode to that of the working electrode. This effectively reduces the IR drop that is often undercompensated.

Advertisement

Synonyms

Luggin-Haber capillary