What Does Shot Blasting Mean?

Shot blasting involves forcibly propelling a stream of abrasive material against a surface using high-pressure air through a nozzle.

Shot blasting is commonly used to:

  • Clean iron, steel, non-cast parts, forgings, etc.
  • Clean mechanical sheets, rods, coils, wire, etc.
  • Prepare surfaces to be painted, coated, etc.
  • Shot peening to alter mechanical properties, increasing resistance to fatigue for springs, gears, etc.
Advertisement

Corrosionpedia Explains Shot Blasting

Shot blasting is used in almost every industry that uses metal, including:

  • Aerospace
  • Automotive
  • Construction
  • Foundry
  • Shipbuilding
  • Rail

Steel surfaces, such as aircraft carriers, ships, petroleum and water storage tanks may be shot blasted to remove rust, non-skid coatings, paint and marine growth. This may be done before these surfaces are coated (or re-coated) for corrosion resistance.