Sling Psychrometer

Last updated: November 23, 2016

What Does Sling Psychrometer Mean?

A sling psychrometer is a hygrometer that can be rotated in the air to make a wet-bulb attain a constant value. It is used to determine the atmospheric humidity in a given area.

Advertisement

Corrosionpedia Explains Sling Psychrometer

A sling psychrometer is used to determine the atmospheric humidity of an environment that surrounds a given metal application.

High moisture levels in the immediate vicinity of a metal can contribute to higher corrosion rates due to the formation of aqueous ions. The use of a sling psychrometer facilitates the proper corrosion prevention methods to be taken in a timely manner depending on the observed moisture levels.