MIL-DTL-5541

Last updated: November 14, 2016

What Does MIL-DTL-5541 Mean?

MIL-DTL-5541 is a military specification related to conversion coatings. This is created through the chemical conversion substance reaction with aluminum and its alloys.

Although MIL-DTL-5541 has been superseded by more recent specifications, it still remains a specification approved by all agencies and departments in the US Department of Defense (DoD). Despite the fact that it was specially created for applications by the DoD, this standard can be used for other applications as well. It has become more popular throughout various fields than its ISO equivalent.

Advertisement

Corrosionpedia Explains MIL-DTL-5541

MIL-DTL-5541 covers all chemical conversion coatings which are known to create protection through chemical reaction with metals like aluminum and aluminum alloy. Such coatings can be classified as:

  • Type 1 – This includes all coatings that have hexavalent chromium. This kind of film usually looks brown or gold, but can be colorless at times.
  • Type 2 – This refers to compositions that contain no hexavalent chromium. This kind of coating appears colorless.
  • Class 1A – This type offers optimal protection to unpainted and painted surfaces against corrosion. This type is thick and typically used as powder coating, paint pre-treatment and final finish.
  • Class 3 – This gives protection from corrosion in cases where low levels of electrical resistance are needed. It is thin and offers low contact resistance with weight lower than corrosion protection.

These coatings are primarily intended for aluminum alloy and plain aluminum, as well as substrates that have not been anodized. These mainly repair aluminum’s anodized coatings. Typically, these are assigned as post treatment to ion-vapor deposition (IVD) type aluminum, mostly found on numerous military platforms like a galvanic inhibitor or an alternative to cadmium.

Types 1 and 2 particularly offer corrosion protection to unpainted surfaces and enhance paint adhesion on aluminum and its alloys. Under MIL-DTL-5541 are coatings that exceed almost all products available commercially, as these are primarily intended for military aircraft.

Advertisement

Synonyms

Military Specification

Chemical Conversion Coatings on Aluminum and Aluminum Alloys