Three-Layer Extruded Polyethylene Coating (3LPE)

Last updated: February 14, 2019

What Does Three-Layer Extruded Polyethylene Coating (3LPE) Mean?

A three-layer extruded polyethylene coating (3LPE) is composed of extruded, three-layer, anti-corrosive steel pipe coatings. The three layers in this type of coating consist of:

  • Bonding agent or copolymer layer
  • Epoxy layer
  • Polypropylene or polyethylene layer
Advertisement

Corrosionpedia Explains Three-Layer Extruded Polyethylene Coating (3LPE)

A three-layer extruded polyethylene coating is used for various types of pipelines including sewer systems, water pipelines, gas pipelines and other channels that are dangerous to water. Polyethylene coatings have been in use to protect buried pipelines from corroding since the 1950s. This type of coating provides higher resistance to insulation than bitumen coatings.

A three-layer extruded polyethylene coating can be applied through sight extrusion and sleeve extrusion. These two methods of applying polyethylene coating were introduced in the 1960s, replacing the sintering technique. It was in the 1980s when 3LPE became very prevalent in the industry.

One advantage of this coating material is that it is ultra-adhesive, even at room temperature. Also, it can be easily cut back as necessary by having the pipelines heated. Furthermore, this material has a very strong chemical resistance that makes it applicable even in the most aggressive environments, including all forms of soil.

The chemical resistance of this coating prevents its corrosion. However, it should be noted that just like many materials, it is also prone to some types of corrosion. Due to this, as early as 1974, testing has been required to determine the aging or corrosion resistance of 3LPE. This is conducted by measuring the temperature with the use of a thermometer at 140°F (60°C). The measure of aging is the melt index, which is set at an initial value of 25%. Over the years, more advanced testing methods have been developed to determine the 3LPE's aging and resistance to corrosion.