How do you identify microbiologically influenced corrosion in water pipelines?

Answer
By Peter Macios | Published: November 26, 2018 | Last updated: January 31, 2022

There are several approaches that can be used to identify microbiologically influenced corrosion (MIC) in pipelines.

Corrosion monitoring using coupons in a bypass rack is one of the most common methods for detection. The coupons can be easily removed and visually inspected for signs of MIC. If a problem is suspected, the coupons can be pulled and sent to a qualified lab for further examination. (Learn more about coupons in How Corrosion Coupon Holders Can Preserve Your Valuable Assets.) Electrochemical probes can also serve a similar function. In addition, observing corrosion rate meter response to system changes, such as an increased feed of biocide, can also aid in diagnosis.

It’s best to monitor the system for biofilm formation and take corrective action early on to prevent MIC from occurring at all. Historically, techniques for sessile bacteria monitoring have been used to grow the biofilms including corrosion coupons, NiCr mesh coupons, beads and biobox panels. Plate counts, dip slides, organism specific cultures, adenosine triphosphate (ATP) measurements and microscopy are used to estimate the propensity for and severity of fouling, the creation of biofilms and the cleanliness of the system.

Free Download: How To Detect Pipe Corrosion in Underground Force Mains, Plus Must-Have Corrosion Detection Equipment

Finally, a visual inspection of system components should not be overlooked in identifying the potential for MIC. For example, significant tuberculation of carbon steel piping would suggest further investigation and nondestructive examination (NDE) testing might be warranted.

Advertisement

Share this

  • Facebook
  • LinkedIn
  • Twitter

Written by Peter Macios | Executive Product Manager of Water Services and Industrial Process at SUEZ Water Technology and Solutions

Peter Macios

Peter Macios is the Executive Product Manager of Water Services and Industrial Process at SUEZ Water Technology and Solutions. Peter provides strategic direction for product development, portfolio management, and go-to-market strategies ensuring sustainability and growth of this industry leading product line.

More Q&As from our experts

Term of the Day

Oil Based Coating

Oil based coatings are those coatings that contain drying oils. Once this coating is applied it reacts with oxygen and the…
Read Full Term

Don't miss the latest corrosion content from Corrosionpedia!

Subscribe to our newsletter to get expert advice and top insights on corrosion science, mitigation and prevention. We create world-leading educational content about corrosion and how to preserve the integrity of the world’s infrastructure and assets.

Resources
Go back to top